MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Mocom (ALBIS) TEDUR® L 9904-1 Polyphenylene Sulphide, 80% iron
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Base Polymer: Polyphenylene Sulphide

Filler/Additive System: 80% iron

Special Features: Increased thermal conductivity, electrostatically dissipating, high density

Market Segment: Automotive, Machinery, Electrical and Electronic

Application Area: Electrical components

Typical Applications: Coil formers/bobbins

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.82 g/ccISO 1183
Storage Temperature <= 30.0 °Cdry, protected from light
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 45.0 MPaISO 527
Elongation at Break 0.40 %ISO 527
 0.60 %deflection at max force; ISO 178
Tensile Modulus 12500 MPaISO 527
Flexural Strength 79.0 MPaISO 178
Flexural Modulus 14300 MPaISO 178
Izod Impact, Unnotched (ISO) 8.00 kJ/m²ISO 180/1U
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.60 W/m-KISO 22007-2
Melting Point 282 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 205 °CISO 75-1/-2
Flammability, UL94 V-2
@Thickness 1.50 mm
 V-0
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 320 - 340 °CInjection molding
Mold Temperature >= 140 °CInjection molding
Drying Temperature 130 - 140 °C
@Time 7200 - 14400 sec
in a dry air (desiccant) dryer
 
Descriptive Properties
Base PolymerPolyphenylene Sulfide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PALBIS8941 / 243000

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.