MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Epoxies, Etc 40-3905 Electrically Conductive Epoxy Adhesive And Coating
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: 40-3905 is an electrically conductive epoxy system designed for applications requiring low temperature cures. 40-3905 will cure at room temperature in 18-24 hours or can be accelerated with mild heat. This is a solvent free epoxy system filled with pure silver. It has outstanding adhesion to plastics, aluminum, copper, magnesium, steel, bronze, nickel, kovar, ceramic, glass, phenolic, and printed circuit boards. 40-3905 can also be thinned with up to 10% Toluol for many coating applications.

Features:

  • Electrically conductive
  • Thermally conductive
  • Room temperature cure
  • Good bond strength

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/ccHardener
 2.98 g/ccResin
Linear Mold Shrinkage 0.0030 in/in
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80 - 85
Flexural Strength 10900 psi
Shear Strength 1200 psiLapshear (Al to Al)
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.00010 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 26.0 µm/m-°C
Thermal Conductivity 8.65 W/m-K
Maximum Service Temperature, Air 135 °C
Minimum Service Temperature, Air -60.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 - 3.00 hour
@Temperature 65.0 °C
 18.0 - 24.0 hour
@Temperature 25.0 °C
Pot Life 45.0 min
@Load 0.100 kg
Shelf Life 12.0 Month
 
Descriptive Properties
Mix Ratio100:5by weight (Resin:Catalyst)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PFEPOX112 / 316789

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.