MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Medalist® MD-16150G Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Medalist MD-16150G XRD1 is a high performance thermoplastic elastomer specifically designed for healthcare and medical applications. Medalist MD-16150G XRD1 is a low hardness, low density, tack-free grade that can be sterilized and is suitable for injection molding.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Chemical Resistant; Ethylene Oxide Sterilizable; Good Colorabiilty; Good Moldability; Good Processability; Good Toughness; Halogen Free; High Elongation; High Flexibility; High Flow; Low Density; Low Hardness; Resilient; Soft; Tack Free

Uses: Disposable Hospital Goods; Medical Devices; Rubber Replacement; Soft Touch Applications; Surgical Instruments

Agency Ratings: ISO 10993 Part 5; ISO 13485

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data.

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.842 g/ccASTM D792
Melt Flow 31 g/10 min
@Load 2.16 kg,
Temperature 150 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore OO 49
@Time 5.00 sec
Injeciton Molded; ASTM D2240
 51
@Time 1.00 sec
Injeciton Molded; ASTM D2240
Tensile Strength at Break 377 psiDie C, 20 in/min; ASTM D412
Tensile Stress at Strain 15.0 psi
@Strain 100 %
Die C, 20 in/min; ASTM D412
 25.0 psi
@Strain 300 %
Die C, 20 in/min; ASTM D412
Elongation at Break 1200 %Die C, 20 in/min; ASTM D412
Tear Strength 48.0 pliDie C, 20 in/min; ASTM D624
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 280 - 310 °F
Middle Barrel Temperature 300 - 330 °F
Front Barrel Temperature 320 - 350 °F
Nozzle Temperature 320 - 350 °F
Melt Temperature 320 - 350 °F
Mold Temperature 80.0 - 120 °F
Back Pressure 25.0 - 100 psi
Cushion 0.150 - 1.00 in
 
Descriptive Properties
AppearanceClear/Transparent
 Colors Available
 Natural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0707 / 237198

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.