MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC NORYL™ Resin PN235 Polyphenylene Ether + PS (PPE+PS) (Americas)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ PN235 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This plate able compression and injection moldable grade exhibits good impact resistance along with low moisture absorption, creep resistance, dimensional stability, and hydrolytic stability. NORYL PN235 resin is an excellent candidate for a variety of plated automotive applications.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/ccASTM D792
Water Absorption 0.10 %
@Time 86400 sec
0.10 %
@Time 24.0 hour
ASTM D570
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 37.0 MPa5370 psi50 mm/min; ASTM D638
Elongation at Break 72 %72 %50 mm/min; ASTM D638
Flexural Strength 55.0 MPa7980 psiyld, 2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 1.82 GPa264 ksi2.6 mm/min, 100 mm span; ASTM D790
Izod Impact Notched 347 J256 ft-lbASTM D256
 133 J
@Temperature -40.0 °C
98.1 ft-lb
@Temperature -40.0 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Arc Resistance 60 - 120 sec60 - 120 secASTM D495
Comparative Tracking Index >= 600 V>= 600 VUL 746A
Hot Wire Ignition, HWI 15 - 30 sec15 - 30 secUL 746A
High Amp Arc Ignition, HAI 30 - 60 arcs30 - 60 arcsUL 746A
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min3.15 - 5.91 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 75.6 µm/m-°C
@Temperature 0.000 - 100 °C
42.0 µin/in-°F
@Temperature 32.0 - 212 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
@Thickness 6.40 mm
234 °F
@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
@Thickness 6.40 mm
219 °F
@Thickness 0.252 in
unannealed; ASTM D648
UL RTI, Electrical 50.0 °C122 °FUL 746B
UL RTI, Mechanical with Impact 50.0 °C122 °FUL 746B
UL RTI, Mechanical without Impact 50.0 °C122 °FUL 746B
Flammability, UL94 HB
@Thickness 1.47 mm
HB
@Thickness 0.0579 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 265 - 295 °C509 - 563 °F
Zone 2 245 - 290 °C473 - 554 °F
Zone 3 255 - 295 °C491 - 563 °F
Melt Temperature 265 - 295 °C509 - 563 °FInjection Molding
Mold Temperature 65.0 - 95.0 °C149 - 203 °F
Drying Temperature 95.0 - 105 °C203 - 221 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 30 - 70 %30 - 70 %
Vent Depth 0.00380 - 0.00510 cm0.00150 - 0.00201 in
Screw Speed 20 - 100 rpm20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82422 / 290369

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.