MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

ExxonMobil Exxon™ Chlorobutyl 5066 Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Exxon™ chlorobutyl rubber is an isobutylene-isoprene copolymer derived from reacting butyl rubber with chlorine in a continuous process. It is structurally similar to Exxon™ bromobutyl rubber and produced through the same halogenation process.  A range of polymer viscosities and cure responses through adjustments in functionality and additives content is available. Compared with regular butyl rubber, Exxon chlorobutyl rubber provides an improved compression set and better resistance to heat, ozone and flex fatigue.

Benefits:  Low permeability to air, gases and moisture

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³
Mooney Viscosity 35 - 45
@Temperature 125 °C
35 - 45
@Temperature 257 °F
ML 1+8. MV 200 or equivalent; ASTM D1646
 
Component Elements PropertiesMetricEnglishComments
Calcium, Ca 0.065 - 0.125 %0.065 - 0.125 %ExxonMobil Method
Chlorine, Cl 1.4 - 1.6 %1.4 - 1.6 %ExxonMobil Method
H2O, Water <= 0.30 %<= 0.30 %ExxonMobil Method
 
Descriptive Properties
Antioxidant (non-staining)0.05 - 0.13wt%. Non-staining. ExxonMobil Method
Cure Characteristics0.0 - 4.0min. ts2. ASTM D2084 (mod). Rheometer ODR 2000 standard compound: ASTM D3958 (mod).
 1.0 - 7.0min. t'50. ASTM D2084 (mod). Rheometer ODR 2000 standard compound: ASTM D3958 (mod).
 11.5 - 20.5dN*m. ML. ASTM D2084 (mod). Rheometer ODR 2000 standard compound: ASTM D3958 (mod).
 39.0 - 53.0dN*m. MH. ASTM D2084 (mod). Rheometer ODR 2000 standard compound: ASTM D3958 (mod)
 7.0 - 13.0min. t'90. ASTM D2084 (mod). Rheometer ODR 2000 standard compound: ASTM D3958 (mod).

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEX98815 / 238200

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.