MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Leaded Commercial Bronze, UNS C31400, OS050 Temper, Rod
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: Nominal Grain Size 0.050 mm

Fabrication Properties: Excellent Suitability – Soldering; Good Suitability – Brazing, Capacity for Being Cold Worked; Fair Suitability – Butt Weld; Poor Suitability – Capacity for Being Hot Formed

Typical uses: Door Knobs; Connectors for Wire and Cable; Electrical Plug Type Connectors; Nuts; Screws; Pickling Crates; Pickling Fixtures; Pickling Racks; Screw Machine Parts

Applicable Specifications: Bar – ASTM B140/B140M; Rod – ASTM B140/B140M; Shapes - ASTM B140/B140M; Valves – MILITARY MIL-V-18436

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.319 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell F 55
@Thickness 25.4 mm
Tensile Strength 37.0 ksi
@Thickness 25.4 mm
Tensile Strength, Yield 12.0 ksi
@Thickness 25.4 mm
0.5% Ext
Elongation at Break 45 %
@Thickness 25.4 mm
Tensile Modulus 17000 ksi
Modulus of Rigidity 6400 ksi
Poissons Ratio 0.33Calculated
Machinability 80 %
Shear Strength 24.0 ksi
@Thickness 25.4 mm
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000410 ohm-cm42% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.2 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 104 BTU-in/hr-ft²-°F
Melting Point 1850 - 1900 °F
Solidus 1850 °F
Liquidus 1900 °F
Annealing Point 800 - 1200 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 87.5 - 90.5 %
Iron, Fe <= 0.10 %
Lead, Pb 1.3 - 2.5 %
Nickel, Ni <= 0.70 %
Zinc, Zn 6.2 - 11.2 %As Balance

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC31400x1 / 292907

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.