MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC Lexan® 9945A PC (Europe-Africa-Middle East)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Lexan* resin 9945A Polycarbonate (PC)is a non-filled, injection moldable grade. This non-chlorinated, non-brominated PC has an UL-94 V0 rating at 1.8 mm. Lexan resin 9945A is available in clear transparent only and is a general-purpose resin intended for thin wall applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Density 1.20 g/ccISO 1183
Moisture Absorption 0.150 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.35 %ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC Method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC Method
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
Melt Index of Compound 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
MVR [cm^3/10 min]; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, H358/30 95.0 MPaISO 2039-1
Tensile Strength at Break 65.0 MPa50 mm/min; ISO 527
 66.0 MPaType I, 50 mm/min; ASTM D638
Tensile Strength, Yield 63.0 MPa50 mm/min; ISO 527
 64.0 MPaType I, 50 mm/min; ASTM D638
Elongation at Break 100 %50 mm/min; ISO 527
 120 %Type I, 50 mm/min; ASTM D638
Elongation at Yield 6.0 %Type I, 50 mm/min; ASTM D638
 6.0 %50 mm/min; ISO 527
Tensile Modulus 2350 MPa1 mm/min; ISO 527
 2380 MPa5 mm/min; ASTM D638
Flexural Yield Strength 90.0 MPa2 mm/min; ISO 178
 102 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2300 MPa2 mm/min; ISO 178
 2450 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 820 J/mASTM D256
 110 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 70.0 kJ/m²80*10*3; ISO 180/1A
 12.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*3; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*3 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 73.0 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 14.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 79.0 J
@Temperature 23.0 °C
ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant 2.7
@Frequency 1e+6 Hz
IEC 60250
 2.7
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 17.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
Dissipation Factor 0.0010
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.010
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 225 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 68.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
 73.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
Thermal Conductivity 0.200 W/m-KISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 136 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
 138 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 125 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
 127 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 141 °CRate B/50; ISO 306
 142 °CRate B/120; ISO 306
 143 °CRate B/50; ASTM D1525
Flammability, UL94 V-2
@Thickness 0.800 mm
UL 94
 V-0
@Thickness 1.80 mm
UL 94
Oxygen Index 35 %ISO 4589
Glow Wire Ignition Temperature 850 °CIEC 60695-2-13
 850 °CIEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 1.00 mm
IEC 60695-2-12
 
Optical PropertiesOriginal ValueComments
Haze 1.0 %
@Thickness 2.54 mm
ASTM D1003
Transmission, Visible 88 %2.54 mm; ASTM D1003
 
Descriptive Properties
Ball Pressure Test, 125°C +/- 2°CPASSESIEC 60695-10-2

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® 6555 Polycarbonate, Injection Grade
SABIC Lexan® 135 PC
SABIC Lexan® 121 PC
LNP Lexan® LC1500N Polycarbonate, 15% Carbon Fiber Reinforced
Covestro Makrolon® 6485 Polycarbonate, Injection Grade

PSABI54711 / 154757

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.