MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Covestro Addigy® FPB 2684 000000 A PC/ABS 3D Printing Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: Optimized for printability. Smooth surface finish. Tough and rigid, impact and heat resistant, cold stable until -30 °C, UV stable. Particularly suitable for outdoor applications e.g. jigs & fixtures in harsh environments.

Information provided by Covestro

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183-1
Melt Flow 18 g/10 min
@Load 1.20 kg,
Temperature 300 °C
18 g/10 min
@Load 2.65 lb,
Temperature 572 °F
(volumetric cm³/10 min)
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 47.0 MPa6820 psi200 mm/min; xy-direction; ISO 527-2
Elongation at Break 12 %12 %200 mm/min; xy-direction; ISO 527-2
Modulus of Elasticity 1.93 GPa280 ksi200 mm/min; xy-direction; ISO 527-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C266 °F50 N; 120 °C/
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FASTM D648
Vicat Softening Point 120 °C248 °F50 N; 120 °C/h; ISO 306
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 270 - 285 °C518 - 545 °F
 
Descriptive Properties
Bed temperature (°C)120
ColorNatural
Printing speed (mm/s)30 to 70

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOVEST1010 / 291047

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.