MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
HB Fuller 42327/52343 Polyurethane Adhesive
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: 42327-52343 is a medium-hardness, semi-flexible two–component polyurethane adhesive designed for bonding applications requiring resilient bonds, non-sag application and enhanced adhesion to flexible substrates. 42327-52343 is suitable for bonding metals, ceramics, natural rubber, thermosetting polymers and select types of unprepared thermoplastic substrates such as ABS, Polycarbonate and Nylon.

Features and Benefits:

  • Excellent bond strength to a wide variety of substrates
  • Low Exotherm
  • Good thermal performance
  • Good chemical resistance
  • Non Sag
  • High Flexibility

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.31 g/cc
Viscosity 16000 cPPart A
 83000 cPPart B
Storage Temperature 16.0 - 27.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65ASTM D2240
Tensile Strength 25.6 MPa50% RH; ASTM D638
Elongation at Break 160 %50% RH; ASTM D638
Shear Strength 4.40 MPaOverlap, ABS, IPA wipe; ASTM D1002
 7.20 MPaOverlap, Nylon 6-6, abraded; ASTM D1002
 13.1 MPaOverlap, Electrogalvanized Steel, IPA wipe; ASTM D1002
 13.8 MPaOverlap, PC, IPA wipe; ASTM D1002
 14.3 MPaOverlap, GFPC, abraded; ASTM D1002
 15.2 MPaOverlap, Aluminum, abraded; ASTM D1002
 20.7 MPaOverlap, Cold Rolled Steel, abraded; ASTM D1002
 22.3 MPaOverlap, Stainless Steel, abraded; ASTM D1002
 24.9 MPaOverlap, E-Coat Steel, IPA wipe; ASTM D1002
 
Processing PropertiesOriginal ValueComments
Cure Time 15.0 minTack Free Time
 2.00 hour
@Temperature <=80.0 °C
Full Cure
 18.0 hour
@Temperature <=25.0 °C
Full Cure
Gel Time 3.00 - 5.00 min
@Load 0.0100 kg
Shelf Life 6.00 Month
 
Descriptive Properties
ColorBlack
ConsistencyThixotropic Paste
Mix Ratio100:100Volume
 100:125Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL062 / 316853

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.