MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Kaowool Rope and Textile
Categories: Ceramic; Oxide

Material Notes: Kaowool textiles are completely asbestos free and possess all the high temperature and superior properties of Kaowool fibers. Ceramic fibers are carded with a blend of organic fibers to form rovings. A reinforcement of glass filament of inconel wire is then introduced and the combination spun to produce the yarns that are the basis of the Kaowool textile range. Yarns and textiles are suitable for a wide range of high temperature sealing and insulating applications. TYPES AVAILABLE: Yarn, cloth, cabled rope(high density), cable rope(low density), rope lagging, twisted rope, webbing, and ladder rope.

Information provided by Morgan Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Classification Temperature (°C)1100Inconel Wire
 1260Alumino Silicate
 550Glass Filament

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMORF7052 / 203351

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.