MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Domo TECHNYL® AR 218 V25 Nylon 66, 25% glass fiber, DRY
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: Polyamide PA66 reinforced with 25% of glass fiber, heat stabilized, containing recycled material.

Available in: Europe and North America

Product Applications: TECHNYL® AR 218 V25 BLACK even if it shows slightly lower and more variable mechanical performances than the virgin prime grade TECHNYL® A 218 V25,can be used in all sectors of industry in less demanding applications and fits the main quality standards of Automotive market. This product is available in black

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.32 g/cc0.0477 lb/in³ISO 1183/A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 125 MPa18100 psiISO 527 Type 1A
Elongation at Break 2.5 %2.5 %ISO 527 Type 1A
Tensile Modulus 7.80 GPa1130 ksiISO 527 Type 1A
Flexural Strength 200 MPa29000 psiISO 178
Flexural Modulus 7.20 GPa1040 ksiISO 178
Izod Impact, Unnotched (ISO) 7.00 kJ/m²3.33 ft-lb/in²ISO 180/1U
Charpy Impact Unnotched 4.00 J/cm²19.0 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FISO 75/Af
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
ISO 1210
 
Processing PropertiesMetricEnglishComments
Feed Temperature 260 - 270 °C500 - 518 °F
Mold Temperature 80.0 - 100 °C176 - 212 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone270-280°C
Mixing Zone280-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® A 218 V25 Natural B PA66, 25% glass fiber, DRY
Domo TECHNYL® eXten D 218CR V33 BLACK Nylon Blend, PA 6.10, 66, Dry
Domo TECHNYL® C 216 V40 PA6, 40% glass fiber, DRY
Envalior Pocan® BF 4130 XF 000000 PBT, 30% Glass Fiber
Envalior Pocan® AF 4130 000000 PBT, 30% Glass Fiber Reinforced

PRHOD546 / 137777

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.