Product Description: LD 319.92 resin is an 8.7% vinyl acetate copolymer film resin. Film made from LD 319.92 exhibits superior impact strength and heat sealability. Availability: Latin America, North America and South America Additive: - Antiblock: No
- Slip: No
- Thermal Stabilizer: Yes
Applications: - Meat Packaging
- Primal Meat Bags
Information provided by ExxonMobil |