MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Nouryon Armostat 300-XE75 Tallow-bis(2-hydroxyethyl) amine
Categories: Other Engineering Material

Material Notes: Semi-permanent, animal-based antistatic additive used in HDPE. A 75% concentration of Armostat 300 on a high-density polyethylene carrier.

Applications: Armostat 300-XE75 is a solid high concentrate consisting of 75% Armostat 300, a semi-permanent, animal based antistat on a high-density polyethylene carrier. Armostat 300 is an internal antistatic additive that can be used in various polymers such as PE, LDPE and PP.

CAS number: 61791-44-4, 9002-88-4

EINECS/ELINCS No.: 263-177-5

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.430 - 0.530 g/cc0.0155 - 0.0191 lb/in³
Density 0.950 g/cc0.0343 lb/in³
 
Thermal PropertiesMetricEnglishComments
Melting Point >= 120 °C>= 248 °F
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.060 %<= 0.060 %
 
Descriptive Properties
AppearanceOff-white granules
Content73-77 %Additive content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY264 / 285787

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.