Borcycle™ EG1217SY is a 15 % mineral filled polypropylene compound containing 25% post-consumer recycled polymer and is intended for injection molding. This material provides very good paintability and impact/stiffness balance. Special Features: - Recycled content
- Paint adhesion
- Low density with good impact/stiffness balance enabling weight reduction
Applications: Borcycle EG1217SY has been developed especially for applications like: - Bumpers
- Rocker panels
- Automotive exterior applications
Values determined on standard injection molded specimens conditioned at 23°C and 50% relative humidity after at least 96 hours storage time. To avoid residual humidity from transport or storage, the material should be pre-dried approximately 2h at 80°C.Information provided by Borealis AG |