MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Norplex-Micarta RM329 Rolled and Molded Rod, Cotton Fabric with Melamine Resin System
Categories: Polymer; Thermoset; Melamine

Material Notes: Rolled and Molded Rods made from a fine weave (linen) cotton fabric impregnated with a melamine resin system. RM329 is used for decorative application simulating the color of Ivory.

Information provided by Norplex Micarta.

Key Words: Cotton Fiber, Melamine
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.39 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 89.0
Tensile Strength 9200 psiCondition A
Flexural Strength 18000 psiCondition A
Compressive Strength 28500 psiCondition A
 
Thermal PropertiesOriginal ValueComments
UL RTI, Electrical 115 °C
UL RTI, Mechanical with Impact 125 °C
Flammability, UL94 V-1Condition A
 
Processing PropertiesOriginal ValueComments
Moisture Content 2.20 %Condition D; ASTM D-349
 
Descriptive Properties
Rod Diameter0.5 inch (1.3 mm)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNORPM910 / 323347

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.