General Description GD-MITE powders and dispersions are inorganic gadolinium-oxide nanoparticles. GD-MITE-A products are uncoated and hydrophilic. GD-MITE-O products are coated with an organic silane (1-4%) and are hydrophobic. Particles are available in the size range of 10-200 nm. |
Formula: Gd2O3; CAS Number: 12064-62-9 |