MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Radici RADILON® DT RV300RKC2 106 NT PA612, 30% Glass Fiber Reinforced, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Glass Fiber Filler

Material Notes: Description: PA612, 30% glass fiber reinforced injection molding grade. Heat stabilized. Natural color. Suitable for parts requiring high stiffness and good mechanical resistance in direct contact with drinking water and food. Exhibits good dimensional stability, improved hydrolytic stability and very good chemical resistance to disinfectants. Product developed for applications in civil and industrial water management as well as appliances.

Processing: Injection Molding

Delivery Form: Granules

Additives: Release agent

Special Characteristics: Heat stabilized or stable to heat, Hydrolysis Resistance, Food Contact, Drinking Water Contact, UL Listed, Low Moisture Absorption

Industries: Water Management

Regional Availability: North America, Europe, Asia Pacific, South and Central America, Near East/Africa

Information provided by Radici Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.29 g/ccISO 1183
Water Absorption 1.9 %
@Thickness 2.00 mm
Immersion at 23°C; ISO 62
Moisture Absorption 0.700 %
@Thickness 2.00 mm
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cmMelt Temp/Mold Temp/Cavity Pressure: 280/60/60; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cmMelt Temp/Mold Temp/Cavity Pressure: 280/60/60; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 130 MPa5mm/min; ISO 527-2/1A
Elongation at Break 4.1 %5mm/min; ISO 527-2/1A
Tensile Modulus 7900 MPa1mm/min; ISO 527-2/1A
Flexural Strength 205 MPa2mm/min; ISO 178
Flexural Modulus 6000 MPa2mm/min; ISO 178
Charpy Impact Unnotched 80.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 15.0 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cm500V; IEC 60093
Surface Resistance 1.00e+10 ohm500V; IEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 120 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
Melting Point 210 °CISO 11357-1/-3
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 - 290 °C
Mold Temperature 80.0 - 90.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRADICI092 / 313593

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.