MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

DuPont Mobility and Materials TPSiV® 4000-60A Silicone Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: UV stable silicone thermoplastic elastomer with excellent abrasion and scratch resistance.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.025 cm/cm0.025 in/inISO 294-4, 2577
Melt Flow 20 g/10 min
@Load 10.0 kg,
Temperature 190 °C
20 g/10 min
@Load 22.0 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 5.20 MPa754 psiCross direction; ISO 527-1/-2 or ISO 37
Tensile Stress at Strain 2.20 MPa
@Strain 100 %
319 psi
@Strain 100 %
Cross direction; ISO 527-1/-2 or ISO 37
Elongation at Break >= 300 %>= 300 %Cross direction; ISO 527-1/-2 or ISO 37
Flexural Strength 1.51 MPa219 psiISO 178
Flexural Modulus 0.0244 GPa3.54 ksiISO 178
Tear Strength 30.0 kN/m171 plinormal; ISO 34-1
Compression Set 33 %
@Temperature 23.0 °C
33 %
@Temperature 73.4 °F
ISO 815
 87 %
@Temperature 70.0 °C,
Time 86400 sec
87 %
@Temperature 158 °F,
Time 24.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Melt Temperature 170 °C338 °FOptimum, Extrusion
 160 - 180 °C320 - 356 °FRange, Extrusion
 190 °C374 °FOptimum, Injection
Mold Temperature 30.0 °C86.0 °FOptimum, Injection
 20.0 - 40.0 °C68.0 - 104 °FInjection
Drying Temperature 85.0 °C185 °FInjection
 85.0 °C185 °FExtrusion
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourExtrusion, Dehumidified Dryer
 2.00 - 4.00 hour2.00 - 4.00 hourInjection, Dehumidified Dryer
 
Descriptive Properties
CompatibilityAcrylic Polymers
 Polycarbonate
 Styrenics
Drying RecommendedyesInjection
Max. screw tangential speed (m/s)0.4Injection
PolymerTPV

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSX4902 / 249181

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.