MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Marco Polo MARPOL EVA 1301 EVA
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: MARPOL® EVA 1301 is a vinyl acetate copolymer with good toughness, flexibility and clarity. Typical applications include laminating and extrusion films.

Recommended Applications: Compounding, freezer film, heat seal layer, liquid packaging, primal meat bags, profile extrusion and stretch film.

Additives: Antiblock – no, Slip – no.

Information provided by Marco Polo International, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.935 g/cc0.0338 lb/in³ASTM D792
Vinyl Acetate Content 13.5 %13.5 %
Melt Flow 0.45 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.45 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 6.55 MPa950 psiASTM D882
Film Tensile Strength at Yield, TD 5.52 MPa800 psiASTM D882
Film Elongation at Break, MD 360 %360 %ASTM D882
Film Elongation at Break, TD 660 %660 %ASTM D882
Flexural Modulus, 1% Secant 80.7 MPa11700 psiMD; ASTM D882
 89.6 MPa13000 psiTD; ASTM D882
Elmendorf Tear Strength MD 66 g66 gASTM D1922
Elmendorf Tear Strength, MD 3.23 g/micron82.0 g/milASTM D1922
Dart Drop Test 710 g1.57 lbASTM D1709
Film Tensile Strength at Break, MD 33.9 MPa4920 psiASTM D882
Film Tensile Strength at Break, TD 34.5 MPa5010 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 76.0 °C169 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 2.4 %2.4 %ASTM D1003
Gloss 80 %80 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMARCO207 / 283804

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.