MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Toyobo Fortron® FX650T6 PPS, 50% Glass/Mineral Reinforced, Impact Modified
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled

Material Notes: Product Description: Forton FX650T6 is a 50% glass-fiber and mineral reinforced grade with improved impact and heat shock resistance.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Filler/Reinforcement: Glass Fiber/Mineral

Additive: Impact Modifier

Features: Impact Modified

Processing Method: Injection Molding

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.70 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0030 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 18900 psiISO 527-2/5
Elongation at Break 2.0 %ISO 527-2/5
Tensile Modulus 1.77e+6 psiISO 527-1
Flexural Strength 26100 psiISO 178
Flexural Modulus 1.74e+6 psiISO 178
Charpy Impact, Notched 4.30 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 62631-3-1
Comparative Tracking Index 100 - 174 VUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 8.30 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 28.0 µin/in-°FISO 11359-2
Melting Point 536 °FISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 518 °FUnannealed; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Processing Temperature 68.0 - 86.0 °FHopper
 626 - 644 °FHot Runner
Feed Temperature 140 - 176 °FInjection
Rear Barrel Temperature 554 - 572 °F
Middle Barrel Temperature 590 - 608 °F
Front Barrel Temperature 626 - 644 °F
Nozzle Temperature 590 - 626 °F
Zone 4 626 - 644 °FInjection
Melt Temperature 626 - 644 °F
Mold Temperature 284 - 320 °F
Drying Temperature 266 - 284 °F
Dry Time 3.00 - 4.00 hour
Screw Speed 50 rpm
@Thickness 55.9 mm
 75 rpm
@Thickness 40.6 mm
 120 rpm
@Thickness 24.9 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHCQ6288 / 310981

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.