MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 7049-T73; 7049-T7352
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 7000 Series Aluminum Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: AA7049-T73; AA7049-T735, UNS A97049; Aluminium 7049-T73 and Aluminium 7049-T7352; Al7049-T73
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.84 g/cc0.103 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 135135AA; Typical; 500 g load; 10 mm ball
Hardness, Knoop 170170Converted from Brinell Hardness Value
Hardness, Rockwell A 50.550.5Converted from Brinell Hardness Value
Hardness, Rockwell B 8282Converted from Brinell Hardness Value
Hardness, Vickers 155155Converted from Brinell Hardness Value
Tensile Strength, Ultimate 517 MPa75000 psiAA; Typical
Tensile Strength, Yield 448 MPa65000 psiAA; Typical
Elongation at Break 12 %
@Diameter 12.7 mm
12 %
@Diameter 0.500 in
AA; Typical
Modulus of Elasticity 71.7 GPa10400 ksiAA; Typical; Average of tension and compression. Compression modulus is about 2% greater than tensile modulus.
Poissons Ratio 0.330.33
Fracture Toughness 24.0 MPa-m½21.8 ksi-in½K(IC) in S-L Direction
 34.0 MPa-m½30.9 ksi-in½K(IC) in L-S Direction
 36.0 MPa-m½32.8 ksi-in½K(IC) in L-T Direction
Shear Modulus 27.6 GPa4000 ksi
Shear Strength 303 MPa44000 psiAA; Typical
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000432 ohm-cm
@Temperature 20.0 °C
0.00000432 ohm-cm
@Temperature 68.0 °F
AA; Typical
 
Thermal PropertiesMetricEnglishComments
CTE, linear  23.4 µm/m-°C
@Temperature 20.0 - 100 °C
13.0 µin/in-°F
@Temperature 68.0 - 212 °F
AA; Typical; average over range
 25.0 µm/m-°C
@Temperature 20.0 - 300 °C
13.9 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.960 J/g-°C0.229 BTU/lb-°F
Thermal Conductivity 154 W/m-K1070 BTU-in/hr-ft²-°FAA; Typical at 77°F
Melting Point 477 - 635.0 °C890 - 1175 °FAA; Typical range based on typical composition for wrought products >= 1/4 in. thickness
Solidus 477 °C890 °FAA; Typical
Liquidus 635.0 °C1175 °FAA; Typical
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 85.7 - 89.5 %85.7 - 89.5 %As remainder
Chromium, Cr 0.10 - 0.22 %0.10 - 0.22 %
Copper, Cu 1.2 - 1.9 %1.2 - 1.9 %
Iron, Fe <= 0.35 %<= 0.35 %
Magnesium, Mg 2.0 - 2.9 %2.0 - 2.9 %
Manganese, Mn <= 0.20 %<= 0.20 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.25 %<= 0.25 %
Titanium, Ti <= 0.10 %<= 0.10 %
Zinc, Zn 7.2 - 8.2 %7.2 - 8.2 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 7050-T7451 (7050-T73651)
Aluminum 7049-T352
Aluminum 7050-T7651
Aluminum 7075-T6; 7075-T651
Aluminum 7050-T74

MA7049T73 / 9572

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.