MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Nouryon Trigonox KSM-C75 Mixture of tert-butyl peroxy-2-ethylhexanoate and 1,1-Di(tertbutylperoxy)- 3,3,5-trimethylcyclohexane, 75% in odorless mineral spirits
Categories: Other Engineering Material

Material Notes: Trigonox KSM-C75 is a peroxide mixture (75% active ingredient in odorless mineral spirits) developed for curing UP-resin-based Hot Press Molding formulations (SMC, DMC, BMC etc) in the temperature range of 100- 150°C.

CAS number: 3006-82-4; 6731-36-8

EINECS/ELINCS No: 221-110-7; 229-782-2

Applications: Trigonox KSM-C75 is a peroxide mixture developed for the cure of UP resin based Hot Press Molding formulations (SMC, DMC, BMC etc) in the temperature range of 100 150°C. With this product a high speed of cure can be achieved. The peroxide is partly based on a perketale and is therefore: especially suitable for pigmented systems. restricted applicable for Low Shrink and Low Profile formulations.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.860 g/cc
Viscosity 8.0 cP
Storage Temperature -20.0 - 20.0 °C
 
Thermal PropertiesOriginal ValueComments
Melting Point -20.0 °C
Decomposition Temperature 40.0 °CSelf-Accelerating Decomposition Temperature
 
Processing PropertiesOriginal ValueComments
Shelf Life 3.00 Month
 
Descriptive Properties
AppearanceClear liquid
Content6.2-6.4 %Active oxygen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY1208 / 286731

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.