MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Amodel® AT-6115 HS PPA, 15% glass fiber
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 20% Glass Fiber Reinforced

Material Notes: 15% glass fiber, impact modified, high flow, hot-water molds, heat stabilized

Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin. This grade was developed for automotive snap-fit electronic connectors. It offers high flow and short molding cycles.

- Black: AT-6115 HS BK 324
- Natural: AT-6115 HS NT

Markets/Uses: Automotive / Automotive E/E / Actuators Bus Bars; Electric Vehicles; Engine Sensors; EV Recharger Connectors; Sensors; Solenoids; Wire Harness Connectors; Fuel Flanges; Rollover Valves

Applications: Automotive Applications; Automotive Electronics; Automotive Under the Hood; Connectors; Housings; Industrial Applications; Industrial Parts; Machine/Mechanical Parts; Metal Replacement; Valves/Valve Parts

Features: Fast Molding Cycle; Good Mold Release; Heat Stabilized; High Elongation; High Flow; Impact Modified; Lubricated

Injection notes: Injection Rate: 2 to 4 in/sec
Holding Pressure: 50% of injection pressure
Storage:
- Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccMethod A; ISO 1183
Water Absorption 0.20 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.010 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.011 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 126 MPaISO 527-2
Tensile Strength 122 MPaASTM D638
Elongation at Break 3.4 %ASTM D638
 4.1 %ISO 527-2
Tensile Modulus 5200 MPaISO 527-2
 5380 MPaASTM D638
Flexural Strength 165 MPaASTM D790
 66.9 MPa
@Temperature 100 °C
ISO 178
 170 MPa
@Temperature 23.0 °C
ISO 178
Flexural Modulus 4410 MPaASTM D790
 2340 MPa
@Temperature 100 °C
ISO 178
 4270 MPa
@Temperature 23.0 °C
ISO 178
Compressive Strength 100 MPaASTM D695
Shear Strength 56.5 MPaASTM D732
Izod Impact, Notched 91.0 J/mASTM D256
Izod Impact, Unnotched 850 J/mASTM D256
Izod Impact, Notched (ISO) 12.0 kJ/m²Type 1, Notch A; ISO 180
Izod Impact, Unnotched (ISO) 55.0 kJ/m²Type 1; ISO 180
Charpy Impact Unnotched 76.0 kJ/m²Type 1, Edgewise; ISO 179
Charpy Impact, Notched 11.0 kJ/m²Type 1, Edgewise, Notch A; ISO 179
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 22.0 µm/m-°C
@Temperature 0.000 - 100 °C
ASTM E831
 30.0 µm/m-°C
@Temperature 100 - 200 °C
ASTM E831
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature 0.000 - 100 °C
ASTM E831
 120 µm/m-°C
@Temperature 100 - 200 °C
ASTM E831
Melting Point 305 °CPeak; ASTM D3418
 305 °CISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 298 °CUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 251 °CUnannealed; ISO 75-2/A
 260 °CAnnealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 316 - 324 °C
Front Barrel Temperature 327 - 332 °C
Melt Temperature 321 - 335 °CInjection
Mold Temperature 66.0 - 93.0 °C
Drying Temperature 110 °C
@Time 14400 sec
Moisture Content 0.030 - 0.060 %Injection
 
Descriptive Properties
AdditiveHeat Stabilizer; Impact Modifier; Lubricant; Mold Release
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack; Natural Color
FormsPellets
ProcessingWater-Heated Mold Injection Molding
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4105 / 279905

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.