MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Hapco DI-PAK™ R-4545/30 Potting and Encapsulating System
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: A very low viscosity potting and encapsulating system with excellent flow and penetration into the most intricate electronic components, without voids or porosity. The R-4545 Series cure to a hard, shiny, high gloss, plastic finish that is free from “blushing” under all humidity conditions. The R-4545 Series is ideal for electrical applications where surface finish and appearance are critical.

Information provided by Hapco, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccASTM D-4669
Viscosity 3600 cPASTM D-4878
Linear Mold Shrinkage 0.0015 - 0.0030 in/inASTM D-2566
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 90ASTM D-2240
Tensile Strength 10000 psiASTM D-638
Elongation at Break 3.0 %ASTM D-638
Modulus of Elasticity 436 ksiASTM D-638
Flexural Strength 11650 psiASTM D-790
Flexural Modulus 497 ksiASTM D-790
Izod Impact, Notched 0.530 ft-lb/inASTM D-256
Izod Impact, Unnotched 0.810 ft-lb/inASTM D-256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 8.20e+13 ohm-cmASTM D-270
Dielectric Constant 4.2
@Frequency 100000 Hz
ASTM D-150
 4.5
@Frequency 1000 Hz
ASTM D-150
Dielectric Strength 565 V/milASTM D-149
Dissipation Factor 0.015
@Frequency 100000 Hz
ASTM D-150
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.50 BTU-in/hr-ft²-°F
Maximum Service Temperature, Inert 168 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 - 4.00 hour
@Thickness 3.17 mm,
Temperature 57.2 °C
Demold
 2.00 - 4.00 hour
@Thickness 3.17 mm,
Temperature 93.3 °C
Demold
Gel Time 40.0 min
@Load 0.100 kg
ASTM D-2971
 
Descriptive Properties
Color (cured)Black
Mix Ratio100:27Weight
 100:33Volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHAPCO043 / 317102

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.