MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Chengdu Letain LTP ZC-1180A PPS
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: For its high rigidity and excellent combination properties, PPS is ideal materials of automobile for light weight. For varied function of parts, PPS for automobile is required to have high rigidity, high stiffness, high toughness, resistance to abrasion, corrosion resistant, resistance to solvent, resistance to temperature leap, resistance to hot water creep deformation, easy to process and good dimensional stability. The structure materials, wear resistant materials, resistant materials, heat leap resistant materials, solvent resistant materials and precise molding materials developed by LETIAN Plastics can meet the increasing need of automobile industry.

Information provided by Chengdu Letain Plastic

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.65 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 180 MPa
Elongation at Break 1.6 %
Flexural Strength 250 MPa
Flexural Modulus 16.8 GPa
Izod Impact, Notched (ISO) 12.5 kJ/m²
Izod Impact, Unnotched (ISO) 65.0 kJ/m²
 
Descriptive Properties
Melt index85 g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHENGLT002 / 255855

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.