MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sandvik 317L-3X1R63 Billet
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes: Sandvik 3X1R63 is an austenitic stainless steel with a high molybdenum content. Significant properties are improved such as general and pitting corrosion resistance in comparison with AISI 316L.

Information provided by Sandvik

ASTM 317L; UNS S31703; EN 1.4438

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 155
Tensile Strength, Ultimate 515 - 690 MPa
Tensile Strength, Yield >= 220 MPa
@Strain 0.2 %
 >= 250 MPa
@Strain 1 %
 >= 110 MPa
@Strain 0.2 %,
Temperature 500 °C
 >= 115 MPa
@Strain 0.2 %,
Temperature 450 °C
 >= 119 MPa
@Strain 0.2 %,
Temperature 400 °C
 >= 123 MPa
@Strain 0.2 %,
Temperature 350 °C
 >= 129 MPa
@Strain 0.2 %,
Temperature 300 °C
 >= 135 MPa
@Strain 1 %,
Temperature 500 °C
 >= 136 MPa
@Strain 0.2 %,
Temperature 250 °C
 >= 140 MPa
@Strain 1 %,
Temperature 450 °C
 >= 144 MPa
@Strain 1 %,
Temperature 400 °C
 >= 144 MPa
@Strain 0.2 %,
Temperature 200 °C
 >= 148 MPa
@Strain 1 %,
Temperature 350 °C
 >= 154 MPa
@Strain 1 %,
Temperature 300 °C
 >= 155 MPa
@Strain 0.2 %,
Temperature 150 °C
 >= 161 MPa
@Strain 1 %,
Temperature 250 °C
 >= 169 MPa
@Strain 1 %,
Temperature 200 °C
 >= 172 MPa
@Strain 0.2 %,
Temperature 100 °C
 >= 180 MPa
@Strain 1 %,
Temperature 150 °C
 >= 196 MPa
@Strain 0.2 %,
Temperature 50.0 °C
 >= 197 MPa
@Strain 1 %,
Temperature 100 °C
 >= 221 MPa
@Strain 1 %,
Temperature 50.0 °C
Elongation at Break >= 35 %
Charpy Impact 60.0 J
@Temperature 270 °C
 60.0 J
@Temperature 196 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.030 %
Chromium, Cr 18.5 %
Iron, Fe 62.6 %As Balance
Manganese, Mn 1.8 %
Molybdenum, Mo 3.1 %
Nickel, Ni 13.5 %
Phosphorus, P <= 0.030 %
Silicon, Si 0.40 %
Sulfur, S <= 0.010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type 317L Stainless Steel, annealed sheet
Carlson 317L Austenitic Stainless Steel
Outokumpu 4438 High Performance Austenitic Stainless Steel
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Molybdenum 317L (UNS S31703)
AISI Type 317L Stainless Steel, annealed tubing

NSANDV161 / 19055

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.