MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Alfa Chemistry Materials Butyl glycidyl ether
Categories: Fluid

Material Notes: Synonyms: 1-TERT-BUTOXY-2,3-EPOXYPROPANE; (TERT-BUTOXYMETHYL)OXIRANE; TERT-BUTYL GLYCIDYL ETHER; TBGE; T-BUTYL GLYCIDYL ETHER; ((1,1-dimethylethoxy)methyl)-oxiran; ((1,1-Dimethylethoxy)methyl)oxirane; [(1,1-dimethylethoxy)methyl]-oxiran

Smiles: CC(C)(C)OCC1CO1

Information provided by Alfa Chemistry Materials.

Vendors: Alfa Chemistry is an ISO 9001:2015 certified supplier of various materials, including: MOFs, coatings, nanomaterials, metals, polymers, carbon fibers, graphite, ceramics, glass, semiconductors, catalysts, carbon nanotubes, fullerene, COFs, molecular sieve, quantum dots, recycled plastics, photonic and optical materials, and magnetic materials, for customers worldwide. Alfa Chemistry also provides custom synthesis services for nearly all kinds of materials and chemicals. Learn more about Alfa Chemistry's high quality products at materials.alfachemic.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.913 g/cc
@Temperature 20.0 °C
0.0330 lb/in³
@Temperature 68.0 °F
Molecular Weight 130.099 g/mol130.099 g/mol"Exact Mass" - Based on Specific Isotopes
 130.19 g/mol130.19 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point -70.0 °C-94.0 °F
Boiling Point 152 °C
@Pressure 0.101 MPa
306 °F
@Pressure 14.7 psi
Flash Point 43.3 °C110 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4171.417(20)
 
Descriptive Properties
Alfa Chemistry Materials CategoryPolymer Science
AppearanceLiquid
CAS Number7665-72-7
EC Number231-640-0
GHS Safety DescriptionS16; S26; S36/37
Hazard statementsXn
H-Bond Acceptor2
H-Bond Donor0
InChIKeySFJRUJUEMVAZLM-UHFFFAOYSA-N
IUPAC Name2-[(2-methylpropan-2-yl)oxymethyl]oxirane
Molecular FormulaC7H14O2
Packing GroupIII
Purity>96.0%(GC)
UN Number3271
WGK Germany3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

ZZALFA2016 / 269849

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.