MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
SABIC ULTEM™ Resin SF2360 Polyetherimide (PEI)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: High flow ULTEM for thin wall application

Features: High Stiffness,Hydrolytic Stability,Chemical Resistance,Low Smoke and Toxicity,Good Mechanicals in Broad Temperature Range,Low Creep Sensitivity,Low Shrinkage,Good metal adhesion,Amorphous,High Strength,High Heat Resistance,Good dimensional stability,Flame Retardant,High Flow

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.53 g/ccASTM D792
Density 1.53 g/ccISO 1183
Water Absorption 0.10 %
@Time 86400 sec
ISO 62-1
Moisture Absorption 0.0200 %Injection Molding
 0.0400 %23°C / 50% RH
Viscosity 40 cP
@Load 10.0 kg,
Temperature 345 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0039 cm/cmSABIC method
Linear Mold Shrinkage, Transverse 0.0047 cm/cmSABIC method
Melt Flow 18 g/10 min
@Load 6.60 kg,
Temperature 337 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 148 MPa5 mm/min; ASTM D638
 152 MPa5 mm/min; ISO 527
Elongation at Break 2.0 %5 mm/min; ASTM D638
 2.0 %5 mm/min; ISO 527
Tensile Modulus 11950 MPa5 mm/min; ASTM D638
Flexural Strength 212 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 9940 MPa1.3 mm/min, 50 mm span; ASTM D790
 9940 MPa2 mm/min; ISO 178
Izod Impact Notched 89.0 JASTM D256
Izod Impact, Notched (ISO) 9.00 kJ/m²80*10*4; ISO 180/1A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 13.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
 15.0 µm/m-°C
@Temperature -40.0 - 150 °C
ASTM E831
CTE, linear, Transverse to Flow 54.0 µm/m-°C
@Temperature -40.0 - 150 °C
ASTM E831
 62.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 208 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
 203 °C
@Thickness 3.20 mm
unannealed; ASTM D648
UL RTI, Electrical 105 °CUL 746B
UL RTI, Mechanical with Impact 105 °CUL 746B
UL RTI, Mechanical without Impact 105 °CUL 746B
Flammability, UL94 V-0
@Thickness 1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 345 - 400 °C
Zone 2 340 - 400 °C
Zone 3 345 - 400 °C
Melt Temperature 350 - 400 °CInjection Molding
Mold Temperature 135 - 165 °C
Drying Temperature 150 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
 24.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82764 / 290711

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.