MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC CYCOLOY™ FR Resin CX2142ME Polycarbonate + ABS (PC+ABS) (Asia)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: CYCOLOY CX2142ME Polycarbonate/Acrylonitrile Butadiene Styrene (PC/ABS) blend is an injection moldable, high flow, non chlorinated/brominated flame retardant grade. It has a UL94 V0@1.2mm and 5VB@2.0mm flame rating. This grade has improved chemical resistance compared to standard PC/ABS blends and is a good candidate for thin wall applications and hospital/medical equipment.

Features: Hydrolytic Stability,Chemical Resistance,Flame Retardant,Thin Wall,Non-Chlorinated,Non-Brominated,Good Mold Release

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccASTM D792
Density 1.19 g/ccISO 1183
Moisture Absorption 0.0400 %Injection Molding
 0.100 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.20 %ISO 62-1
Viscosity 21 cP
@Load 2.16 kg,
Temperature 260 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 22.5 g/10 min
@Load 2.16 kg,
Temperature 260 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 51.0 MPa50 mm/min; ISO 527
 54.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 61.0 MPa50 mm/min; ISO 527
 64.0 MPa50 mm/min; ASTM D638
Elongation at Break 90 %50 mm/min; ASTM D638
 90 %50 mm/min; ISO 527
Elongation at Yield 4.0 %50 mm/min; ASTM D638
 4.0 %50 mm/min; ISO 527
Tensile Modulus 2700 MPa1 mm/min; ISO 527
 2900 MPa50 mm/min; ASTM D638
Flexural Strength 100 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 100 MPayield, 2 mm/min; ISO 178
Flexural Modulus 2500 MPa2 mm/min; ISO 178
 2700 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 600 JASTM D256
 120 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 15.0 kJ/m²80*10*3; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Charpy Impact, Notched 15.0 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 63.0 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Thermal Conductivity 0.200 W/m-KISO 8302
Hot Ball Pressure Test 75.0 °CPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 98.0 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 84.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 90.0 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 102 °CRate B/50; ASTM D1525
 102 °CRate B/120; ISO 306
 102 °CRate B/50; ISO 306
UL RTI, Electrical 90.0 °CUL 746B
UL RTI, Mechanical with Impact 90.0 °CUL 746B
UL RTI, Mechanical without Impact 90.0 °CUL 746B
Flammability, UL94 V-0
@Thickness >=1.20 mm
UL 94
 5VB
@Thickness >=2.00 mm
UL 94
 5VA
@Thickness >=3.00 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 245 - 275 °C
Zone 2 220 - 265 °C
Zone 3 245 - 275 °C
Melt Temperature 245 - 275 °CInjection Molding
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 80.0 - 90.0 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 30 - 80 %
Vent Depth 0.00380 - 0.00760 cm
Screw Speed 40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80020 / 287967

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.