MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Alfa Chemistry Materials Erbium Oxide
Material Notes: Erbium Oxide also called Erbia, an important colorant in glasses and porcelain enamel glazes. High purity Erbium Oxide are widely applied as dopant in making optical fiber and amplifier. It is particularly useful as an amplifier for fiber optic data transfer. Erbium Oxide has a pink color, and is sometimes used as a colorant for glass, cubic zirconia and porcelain. The glass is then often used in sunglasses and cheap jewelry.

Applications: Halide Lamps ;Ceramics; Crystal dopant; Neutron Absorbers; Optical fiber; Phosphors, an important colorant in glasses and porcelain enamel glazes. High purity Erbium Oxide are widely applied as dopant in making optical fiber and amplifier.

Solubility: Insoluble in water, moderately soluble in strong mineral acids

Molecular Formula: Er2O3

Erbium(III) oxide2-8°CAlfa Chemistry Materials product group: Metal

Manufacturer data sheet

Vendors: Alfa Chemistry is an ISO 9001:2015 certified supplier of various materials, including: MOFs, coatings, nanomaterials, metals, polymers, carbon fibers, graphite, ceramics, glass, semiconductors, catalysts, carbon nanotubes, fullerene, COFs, molecular sieve, quantum dots, recycled plastics, photonic and optical materials, and magnetic materials, for customers worldwide. Alfa Chemistry also provides custom synthesis services for nearly all kinds of materials and chemicals. Learn more about Alfa Chemistry's high quality products at materials.alfachemic.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.64 g/cc0.312 lb/in³
Solubility in Water 0.00 %0.00 %Insoluble
Molecular Weight 382.52 g/mol382.52 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 2400 °C4350 °F
 
Descriptive Properties
AppearancePink
CAS Number12061-16-4
Purity99.999% 99.99% 99.9% 99%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

ZZALFA67050 / 303562

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.