MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

BASF Ultradur® B 6550 LN FC PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: Ultradur B 6550 LN FC is a high viscosity PBT extrusion grade approved for food contact.

Applications: Typical applications include semi-finished products, profile and hollow rods.

Information provided by BASF.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³ISO 1183
Moisture Absorption 0.250 %0.250 %50% RH; ISO 62
Water Absorption at Saturation 0.40 %0.40 %ISO 62
Viscosity Test 160 cm³/g1.60 dl/gISO 1628
Linear Mold Shrinkage, Flow 0.019 cm/cm0.019 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.022 cm/cm0.022 in/inISO 294-4
Melt Flow 9.5 g/10 min
@Load 2.16 kg,
Temperature 250 °C
9.5 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 56.0 MPa8120 psiISO 527
Elongation at Break >= 50 %>= 50 %Nominal; ISO 527
Elongation at Yield 3.5 %3.5 %ISO 527
Tensile Modulus 2.60 GPa377 ksiISO 527
Flexural Strength 76.0 MPa11000 psiISO 178
Flexural Modulus 2.03 GPa294 ksiISO 178
Charpy Impact Unnotched  22.0 J/cm²
@Temperature -30.0 °C
105 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched  0.520 J/cm²
@Temperature 23.0 °C
2.47 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 0.530 J/cm²
@Temperature -30.0 °C
2.52 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant  3.2
@Frequency 1e+6 Hz
3.2
@Frequency 1e+6 Hz
IEC 60250
 3.4
@Frequency 100 Hz
3.4
@Frequency 100 Hz
IEC 60250
Dissipation Factor  0.0019
@Frequency 100 Hz
0.0019
@Frequency 100 Hz
IEC 60250
 0.0219
@Frequency 1e+6 Hz
0.0219
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 475 V475 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 90.0 - 150 µm/m-°C50.0 - 83.3 µin/in-°F
Melting Point 223 °C433 °FISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 135 °C275 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FISO 75
 
Processing PropertiesMetricEnglishComments
Adapter Temperature 225 °C437 °F
Die Temperature 215 °C419 °F
Melt Temperature 230 - 290 °C446 - 554 °F
Drying Temperature 100 - 120 °C
@Time 14400 sec
212 - 248 °F
@Time 4.00 hour
Moisture Content <= 0.040 %<= 0.040 %
 
Descriptive Properties
Compression Ratio3:1
Extruder250/240/230°C
L/D Ratio20:1
Screw Parameters3 to 4 flightsTransition Section
 45 percentMetering Section

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASF8914 / 254872

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.