MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mocom (ALBIS) ALTECH® PA66 ECO 1000/561 Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Impact Grade

Material Notes: Base Polymer: Polyamide 66

Special Features: Impact modified, contains recycled material

Market Segment: Automotive, Building and Construction, various

Application Area: Fixtures/fittings, transport systems, various

Typical Applications: Housing and automotive trim unpainted, fixing elements, cable ties, various

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ISO 1183
Maximum Moisture Content 0.150.15
Linear Mold Shrinkage, Flow 0.014 - 0.018 cm/cm
@Time 86400 sec
0.014 - 0.018 in/in
@Time 24.0 hour
ISO 294-4
Linear Mold Shrinkage, Transverse 0.016 - 0.020 cm/cm
@Time 86400 sec
0.016 - 0.020 in/in
@Time 24.0 hour
ISO 294-4
Melt Flow 80 g/10 min
@Load 5.00 kg,
Temperature 275 °C
80 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
Storage Temperature <= 30.0 °C<= 86.0 °Fdry, protected from light
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 55.0 MPa7980 psiISO 527
Elongation at Break 25 %25 %ISO 527
Tensile Modulus 2.60 GPa377 ksiISO 527
Flexural Strength 95.0 MPa13800 psiISO 178
Flexural Modulus 2.50 GPa363 ksiISO 178
Charpy Impact Unnotched NBNBISO 179/1eU
Charpy Impact, Notched  0.500 J/cm²
@Temperature -40.0 °C
2.38 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eA
 0.800 J/cm²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FISO 75-1/-2
Vicat Softening Point 200 °C392 °FB50; ISO 306
Flammability, UL94 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 - 290 °C518 - 554 °FInjection molding
Mold Temperature 40.0 - 80.0 °C104 - 176 °FInjection molding
Drying Temperature 80.0 °C
@Time 7200 - 43200 sec
176 °F
@Time 2.00 - 12.0 hour
 
Descriptive Properties
Base PolymerPolyamide 66

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay AB40N Breather fabric
Solvay AB33N Breather fabric
Solvay 51789 Nylon 6.6
Overview of materials for Nylon 66/6
Overview of materials for Nylon 66, Unreinforced

PALBIS8283 / 242342

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.