MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ascend Performance Materials Vydyne® AG10 Nylon PA66-GF50
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled

Material Notes: Vydyne AG10 is a 50% glass fiber reinforced PA66 for injection molded applications.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.58 g/cc0.0571 lb/in³DAM; ISO 1183
Moisture Absorption at Equilibrium 0.70 %0.70 %DAM to 50% RH; ISO 62
Water Absorption at Saturation 2.5 %2.5 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 210 MPa30500 psiDAM; ISO 527-2
Elongation at Break 3.0 %3.0 %DAM; ISO 527-2
Tensile Modulus 14.8 GPa2150 ksiDAM; ISO 527-2
Flexural Strength 310 MPa45000 psiDAM; ISO 178
Flexural Modulus 13.8 GPa2000 ksiDAM; ISO 178
Izod Impact, Notched (ISO)  13.0 kJ/m²
@Temperature -40.0 °C
6.19 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 180/1A
 13.0 kJ/m²
@Temperature -30.0 °C
6.19 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
 15.0 kJ/m²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
Charpy Impact Unnotched 14.0 J/cm²
@Temperature 23.0 °C
66.6 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm
@Thickness 1.00 mm
1.00e+16 ohm-cm
@Thickness 0.0394 in
DAM; IEC 60093
Comparative Tracking Index 500 V
@Thickness 3.00 mm
500 V
@Thickness 0.118 in
IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 19.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 35.0 - 55.0 °C
10.6 µin/in-°F
@Thickness 0.0787 in,
Temperature 95.0 - 131 °F
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 71.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
39.4 µin/in-°F
@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
DAM; ISO 11359-2
UL RTI, Electrical  65.0 °C
@Thickness 0.750 mm
149 °F
@Thickness 0.0295 in
UL 746
 65.0 °C
@Thickness 3.00 mm
149 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical with Impact  65.0 °C
@Thickness 0.750 mm
149 °F
@Thickness 0.0295 in
UL 746
 65.0 °C
@Thickness 3.00 mm
149 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact  65.0 °C
@Thickness 0.750 mm
149 °F
@Thickness 0.0295 in
UL 746
 65.0 °C
@Thickness 3.00 mm
149 °F
@Thickness 0.118 in
UL 746
Flammability, UL94  HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
Oxygen Index 27 %27 %DAM; EN ISO 4589-2
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 260 - 280 °C500 - 536 °FInjection
Middle Barrel Temperature 270 - 280 °C518 - 536 °FInjection
Front Barrel Temperature 270 - 290 °C518 - 554 °FInjection
Melt Temperature 270 - 290 °C518 - 554 °FInjection
Mold Temperature 60.0 - 90.0 °C140 - 194 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 4.00 hour4.00 hourInjection
Moisture Content 0.20 %0.20 %Injection
 
Descriptive Properties
AdditiveHeat Stabilizer
 Release agent
Agency RatingsISO, 1043 PA66 GF50
AppearanceNatural Color
FeaturesGood Stiffness
 Good Strength
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASCE8807 / 293376

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.