MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Selenis CALIMA CA 360 Polymer for CPET Trays
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Selenis Calima CA 360 is a polymer that is uniquely suited for the production of CPET trays, a package that can be used in traditional as well as microwave ovens. This solution delivers the easy meal preparation advantages expected by consumers and is suitable for either chilled or frozen products. Make products eye-catching from store to table, with the excellent optics of Selenis Calima CA 360, whilst delivering consistent barrier properties to extend shelf life. Trays produced with Selenis Calima CA 360 can be MAP or vacuum processed, as well as post-pasteurized. CPET food convenience and service trays made with Selenis Calima CA 360 offer convenient properties for consumers, such as: temperature, shatter and fat resistance, preserving the contents of the package and granting consumers the expected taste experience. Selenis Calima CA 360 is available with different viscosities ranging from 0.74 to 1.15.

Information provided by Selenis.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Moisture Absorption at Equilibrium <= 0.20 %
Viscosity Test 72 - 76 cm³/gIntrinsic; ISO 1628-5
 87 - 91 cm³/gIntrinsic; ISO 1628-5
 93 - 97 cm³/gIntrinsic; ISO 1628-5
 96 - 100 cm³/gIntrinsic; ISO 1628-5
 103 - 107 cm³/gIntrinsic; ISO 1628-5
 106 - 110 cm³/gIntrinsic; ISO 1628-5
 113 - 117 cm³/gIntrinsic; ISO 1628-5
ASTM Color <= 1.0b*; ASTM D6290
 >= 85L*; ASTM D6290
 
Chemical PropertiesOriginal ValueComments
Acetaldehyde <= 1.00 ppmASTM F2013
 
Thermal PropertiesOriginal ValueComments
Melting Point 248 - 258 °C
 
Processing PropertiesOriginal ValueComments
Melt Temperature 285 - 295 °C
Drying Temperature 175 °C
@Time 14400 - 21600 sec
Moisture Content <= 0.0040 %dried
Dew Point -40.0 °C
 
Descriptive Properties
Food Approval PharmacopeiaYes
Particle size320 ± 50 mg/20 chips
Pellet ShapeCylindrical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSELE913 / 243411

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.