MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Carbon Printers EPU 44 Biobased Elastomer for 3D Printing
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoset; Epoxy

Material Notes: 2 part liquid. Available in gray or white.

EPU 44 is production-scale, resilient elastomer that is highly resilient, tear resistant, and has a 40% bio-based formulation. EPU 44 enables lighter lattices than EPU 41 when designed with equivalent stiffness, requiring less material. EPU 44 has a higher green strength as well, allowing for more printable geometries. EPU 44 prints faster than EPU 41, and its higher green strength helps protect yield of delicate designs.

Information provided by Carbon®

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccLiquid, Part B
 1.030 g/ccLiquid, Mixed; ASTM D792
 1.03 g/ccSolid
 1.05 g/ccLiquid, Part A
Viscosity 80 cP
@Temperature 25.0 °C
Liquid, Part B
 6700 cP
@Temperature 25.0 °C
Liquid, Mixed
 8600 cP
@Temperature 25.0 °C
Liquid, Part A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 78Instant
 77
@Time 5.00 sec
Tensile Strength at Break 275 MPaDie C; 500 mm/min; ASTM D412
Tensile Strength, Ultimate 24.0 MPaDie C; 500 mm/min; ASTM D412
Elongation at Yield 5.0 %Die C; 500 mm/min; ASTM D412
50% Modulus 4.00 MPa
@Strain 50 %
Die C; 500 mm/min; ASTM D412
100% Modulus 8.00 MPa
@Strain 100 %
Die C; 500 mm/min; ASTM D412
200% Modulus 20.0 MPa
@Strain 200 %
Die C; 500 mm/min; ASTM D412
Flex Crack Resistance >= 100000
@Temperature 23.0 °C
Cycles Ross Flexing Fatigue Unnotched; no Propagation; ASTM D1052
 >= 100000
@Temperature -10.0 °C
Ross Flexing Fatigue; Notched; no Propagation; ASTM D1052
Tear Strength 35.0 kN/mDie C; ASTM D624
Abrasion 70mm3 Relative Abrasion Loss; ISO -4649 A
Compression Set 25 %
@Temperature 23.0 °C,
Time 259000 sec
ASTM D395-B
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.1e+11 ohm-cmASTM D257
Dielectric Constant 4.26
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 17.0 kV/mmASTM D149
Dissipation Factor 0.0368
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg -5.00 °CDMA tan δ; ASTM D4065
 
Descriptive Properties
ColorBlack
Part A:B Mass Ratio11.4 : 1White
 12.0 : 1Gray
Part A:B Volume Ratio10.3 : 1White
 10.8:1Gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCARBP009c / 295532

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.