MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Go Yen Chemical GY-FRTM Halogenated Flame Retardant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Long term life time; Well Compatibility; High Stability; Non-toxic and odorless; Do not contain heavy metals

Advantages:

  • Can give resin excellent fireproof ability
  • Can add in thermosetting or thermoplastic product
  • With outstanding opacity, can use in various transparent fireproof products
  • Can provide products prominent soft ability
  • Compare to traditional inorganic ore type flame retardant, GY-FR-TM would not affect the physical property and strength of resin and rubber
  • With excellent dispersion and soluble ability
  • Enhances the oxygen index of material
  • GY-FR-TM is outstanding processed-type flame retardant
  • With excellent water and oil resistance
  • With good electrical insulating ability
Applications:
  • Thermal setting resin: epoxy resin, phenol resin, unsaturated resin, polyester resin, acrylic resin, etc.
  • Coating and various resin: flame retardant coating, powder coating, acrylic product required flame retardant, polyurethane resin, PMMA, latex resin, adhesive related product
  • Thermoplastic plastic : PP, POLYOLIFIN, PET, NYLON, POM, engineering plastic, etc.
  • Rubber and Elastomer industry: All kinds of nature and synthetic rubber: TPE, SBS, SEBS
  • Various of foam and flame retard foaming products
  • Polyamide: polyamide 66, 6, 11, 12
  • Polyurethanes Type(TPU, PU RESIN ) Electronic products made from TPU: Switch, connector, covering

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 - 1.20 g/cc0.0426 - 0.0434 lb/in³
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.10 %<= 0.10 %
 
Descriptive Properties
AppearanceWhite flaky crystal powder
Freezing point50°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN042 / 266350

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.