MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) KetaSpire® KT-880 GF30 PEEK, 30% glass fiber
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Glass Fiber Filled

Material Notes: 30% glass fiber, high melt flow for injection molding

KetaSpire® KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire® PEEK resin. Reinforcement also affords greater mechanical robustness in structural applications, particularly those with service temperatures approaching 300°C.

KetaSpire® PEEK is produced to the highest industry standards and is characterized by a distinct combination of properties, which include excellent wear resistance, best-in-class fatigue resistance, ease of melt processing, high purity and excellent chemical resistance to organics, acids and bases.

These properties make it well-suited for applications in healthcare, transportation, electronics, chemical processing and other industrial uses.

- Beige: KT-880 GF30 BG 20
- Black: KT-880 GF30 BK 95

Markets/Uses: Aircraft / Mechanical & Structural Applications / Brackets and Hinges; Aircraft / Mechanical & Structural Applications / Electrical Connectors; Aircraft / Mechanical & Structural Applications / Environmental Control System Components; Aircraft / Mechanical & Structural Applications / Fan Impeller; Aircraft / Mechanical & Structural Applications / Handles; Aircraft / Mechanical & Structural Applications / Mounting Support Rails; Aircraft / Mechanical & Structural Applications / Seals; Aircraft / Mechanical & Structural Applications / Spuds; Aircraft / Mechanical & Structural Applications / Stock Shapes for Prototyping; Aircraft / Mechanical & Structural Applications / Support Brackets; Aircraft / Mechanical & Structural Applications / Thrust Washers; Films / High Temperature Films / Brackets and Hinges; Films / High Temperature Films / Electrical Connectors; Films / High Temperature Films / Environmental Control System Components; Films / High Temperature Films / Fan Impeller; Films / High Temperature Films / Handles; Films / High Temperature Films / Mounting Support Rails; Films / High Temperature Films / Seals; Films / High Temperature Films / Spuds; Films / High Temperature Films / Thrust Washers; Healthcare / Medical Devices / Case Handles and Brackets; Healthcare / Medical Devices / Dental Instruments; Healthcare / Medical Devices / Medical Reusable; Healthcare / Medical Devices / Medical/Healthcare Applications; Healthcare / Medical Devices / Orthopedics; Healthcare / Medical Devices / Packaging, Rigid Medical; Healthcare / Medical Devices / Sizing Trials; Healthcare / Medical Devices / Surgical Instruments; Miscellaneous / Industrial / Compressor Components; Oil & Gas / Down Hole / Back-Up Seal Rings; Oil & Gas / Down Hole / Compressor Components; Oil & Gas / Down Hole / Compressor Plates; Oil & Gas / Down Hole / Down Hole Connectors; Oil & Gas / Down Hole / Electrical Connectors; Oil & Gas / Down Hole / Motor End Plate; Oil & Gas / Down Hole / Poppets

Applications: Aircraft Applications; Connectors; Dental Applications; Electrical/Electronic Applications; Film; Hospital Goods; Industrial Applications; Medical Devices; Medical/Healthcare Applications; Oil/Gas Applications; Pump Parts; Seals; Surgical Instruments

Features: Autoclave Sterilizable; Biocompatible; Chemical Resistant; E-beam Sterilizable; Ethylene Oxide Sterilizable; Fatigue Resistant; Flame Retardant; Good Dimensional Stability; Good Sterilizability; Heat Sterilizable; High Flow; High Heat Resistance; High Stiffness; High Strength; Radiation (Gamma) Resistant; Radiation Sterilizable; Radiotranslucent; Steam Resistant; Steam Sterilizable

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.53 g/ccASTM D792
Water Absorption 0.10 %
@Time 86400 sec
ASTM D570
Viscosity 350 cP
@Shear Rate 1000 1/s,
Temperature 400 °C
Melt; ASTM D3835
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
@Thickness 3.18 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.013 - 0.015 cm/cm
@Thickness 3.18 mm
ASTM D955
Melt Flow 14 g/10 min
@Load 2.16 kg,
Temperature 400 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 105ASTM D785
Tensile Strength 162 MPaASTM D638
Tensile Strength, Yield 174 MPaType 1A, 5 mm/min; ISO 527-2
Elongation at Break 3.1 %5.0 mm/min; ASTM D638
 3.1 %Type 1A, 5 mm/min; ISO 527-2
Tensile Modulus 10800 MPa5.0 mm/min; ASTM D638
 11200 MPa1 mm/min, Type 1A; ISO 527-2
Flexural Strength 239 MPaISO 178
 260 MPaASTM D790
Flexural Modulus 10500 MPaASTM D790
 10600 MPaISO 178
Compressive Strength 183 MPaASTM D695
Shear Strength 94.4 MPaASTM D732
Izod Impact, Notched 69.0 J/mASTM D256
Izod Impact, Unnotched 850 J/mASTM D256
Izod Impact, Notched (ISO) 11.0 kJ/m²ISO 180
Izod Impact, Unnotched (ISO) 62.0 kJ/m²ISO 180
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.80e+17 ohm-cmASTM D257
Surface Resistance >= 1.90e+17 ohmASTM D257
Dielectric Constant 3.49
@Frequency 1e+6 Hz
ASTM D150
 3.53
@Frequency 1000 Hz
ASTM D150
 3.53
@Frequency 60 Hz
ASTM D150
Dielectric Strength 16.0 kV/mm
@Thickness 3.00 mm
ASTM D149
Dissipation Factor 0.0020
@Frequency 1000 Hz
ASTM D150
 0.0020
@Frequency 60 Hz
ASTM D150
 0.0040
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 19.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
ASTM E831
Specific Heat Capacity 1.28 J/g-°C
@Temperature 50.0 °C
ASTM C351
 1.70 J/g-°C
@Temperature 200 °C
ASTM C351
Thermal Conductivity 0.300 W/m-KASTM C177
Melting Point 343 °CPeak; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 315 °CAnnealed; ASTM D648
Glass Transition Temp, Tg 147 °CDSC
Flammability, UL94 V-0
@Thickness 0.800 mm
 V-0
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 365 °C
Middle Barrel Temperature 371 °C
Front Barrel Temperature 377 °C
Nozzle Temperature 382 °C
Mold Temperature 177 - 204 °C
Drying Temperature 150 °C
@Time 14400 sec
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorLight Beige
FormsPellets
Injection RateFast
ProcessingInjection Molding; Machining; Profile Extrusion
RoHS ComplianceYes
Screw Compression Ratio2.5:1.0 to 3.5:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4341 / 280141

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.