MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
ITW Plexus® A0420/MA420 Methacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: Plexus® AO420 is a two-part methacrylate adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies. Combined at a 10:1 ratio, AO420 is a rapid-curing system. Plexus AO420 is the standard choice for composite bonding applications in the transportation industry because it requires virtually no surface preparation. In addition, this product provides a unique combination of excellent fatigue endurance, outstanding impact resistance, and superior toughness. Plexus AO420 is available in amber, blue, or black colors and is supplied ready-to-use to be dispensed as a non-sagging gel.

Excellent chemical resistance to : hydrocarbons, acids and bases (pH 3-10), salt solutions. Susceptible to: polar solvents, strong acids and bases. Recommended for: ? ABS? Acrylics? FRP? Gel coats? Steel (Exterior applications require the use of coatings or primers that inhibit oxidation of the steel.)  ? PVC? Polyesters (including DCPD modified)? Aluminum*? Steel, Stainless? Styrenics? Urethanes (general)? Vinyl Esters

Color: off white/amber (adhesive), off white, blue, and black (activator).

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.10 lb/galadhesive. Uncured.
 8.20 lb/galCured
 8.80 lb/galActivator. Uncured.
Volatile Organic Compounds (VOC) Content <= 20 g/lDuring cure
Viscosity 35000 - 80000 cP
@Temperature 22.2 °C
Activator
 100000 - 125000 cP
@Temperature 22.2 °C
Adhesive.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 2700 - 3000 psiASTM D638
Elongation at Break 30 - 50 %ASTM D638
Tensile Modulus 75000 - 100000 psiASTM D638
Adhesive Bond Strength 3000 - 3800 psiLap Shear Cohesive Strength; ASTM D1002
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air -67.0 °F
Flash Point 51.0 °F
 
Processing PropertiesOriginal ValueComments
Working Life 4.00 - 6.00 min
@Temperature 23.3 °C
Shelf Life 7.00 MonthB Side Back
 7.00 MonthBlack in Cartridges
 10.0 MonthStandard Colors in cartridges
 10.0 MonthActivator (B side)
 13.0 MonthAdhesive (A side)
 
Descriptive Properties
Fixture Time (mins)18 to 2274°F cure. Varies with bond gap and temperature.
Gap Filling (in)0.03 to 0.375Room temperature cure.
Mix Ratio by volume10 to 1Adhesive to Activator. Room temperature
Mix Ratio by weight9.1 to 1.0Adhesive to Activator. Room temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWP9001 / 239511

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.