MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Mitsubishi Chemical Advanced Materials Ketron® CA30 PEEK SP Polyetheretherketone, 30% Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: This 30% carbon fiber reinforced grade combines even higher stiffness, mechanical strength and creep resistance than Ketron® GF30 PEEK SP with an optimum wear resistance. Moreover, compared with unreinforced PEEK, the carbon fibers considerably reduce thermal expansion and provide 3.5 times higher thermal conductivity – dissipating heat from the bearing surface faster, improving bearing life and pressure-velocity capabilities.

Vendors: TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.41 g/cc1.41 g/ccISO 1183-1
Water Absorption <= 0.050 %
@Time 86400 sec
<= 0.050 %
@Time 24.0 hour
ISO 62
Water Absorption at Saturation 0.35 %0.35 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 102102ISO 2039-2
Tensile Strength 135 MPa19600 psiISO 527-1/-2
Elongation at Break 1.5 %1.5 %ISO 527-1/-2
Modulus of Elasticity 11.0 GPa1600 ksiISO 527-1/-2
Flexural Strength 220 MPa31900 psiISO 178
Compressive Strength  80.0 MPa
@Strain 1 %
11600 psi
@Strain 1 %
ISO 604
 150 MPa
@Strain 2 %
21800 psi
@Strain 2 %
ISO 604
 200 MPa
@Strain 5.0 %
29000 psi
@Strain 5.0 %
ISO 604
Charpy Impact Unnotched 2.50 J/cm²11.9 ft-lb/in²ISO 179-1/1eU
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 10000 - 1.00e+6 ohm10000 - 1.00e+6 ohmANSI/ESD STM 11.11
 
Thermal PropertiesMetricEnglishComments
CTE, linear  25.0 µm/m-°C
@Temperature 23.0 - 100 °C
13.9 µin/in-°F
@Temperature 73.4 - 212 °F
ASTM D696
 25.0 µm/m-°C
@Temperature 23.0 - 150 °C
13.9 µin/in-°F
@Temperature 73.4 - 302 °F
ASTM D696
 55.0 µm/m-°C
@Temperature >=150 °C
30.6 µin/in-°F
@Temperature >=302 °F
ASTM D696
Thermal Conductivity 0.920 W/m-K6.38 BTU-in/hr-ft²-°F
Melting Point 340 °C644 °F10°C / min; ISO 11357-1/-3
Maximum Service Temperature, Air 250 °C482 °F20,000 hours
Deflection Temperature at 1.8 MPa (264 psi) 160 °C320 °FISO 75-1/-2
Minimum Service Temperature, Air -20.0 °C-4.00 °F
Flammability, UL94 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

P1SM936 / 291093

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.