MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Corning PHOTOGRAY 16 High Index Photochromic crown glass
Categories: Ceramic; Glass; Optical

Material Notes: Application : Ophthalmic lenses : Single vision, G&P progressive addition.

Information provided by Corning Incorporated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.70 g/cc
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.00 µm/m-°C
Softening Point 685 °C
Annealing Point 530 °C
Strain Point 685 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.59629
@Wavelength 656.3 nm
Line: C; Hydrogen
 1.59694
@Wavelength 643.8 nm
Line: C'; Cadmium
 1.60050
@Wavelength 587.6 nm
Line: d; Helium
 1.60151
@Wavelength 486.1 nm
Line: F; Hydrogen
 1.60387
@Wavelength 546.1 nm
Line: e; Mercury
 1.61123
@Wavelength 480 nm
Line: F'; Cadmium
Abbe Number 42ve
 42.2vd
Transmission, Visible 31 %
@Wavelength 380 - 500 nm,
Thickness 2.00 mm
Blue light transmission factor, Darkened
 32 %
@Wavelength 380 - 780 nm,
Thickness 2.00 mm
Luminous, Darkened
 77 %
@Wavelength 380 - 500 nm,
Thickness 2.00 mm
Blue light transmission factor, Heat Faded
 88 %
@Wavelength 380 - 780 nm,
Thickness 2.00 mm
Luminous, Heat Faded
UV Transmittance <= 0.10 %
@Thickness 2.00 mm
Solar UV-B transmission factor, Heat Faded
 <= 0.10 %
@Thickness 2.00 mm
Solar UV-B transmission factor, Darkened
 1.5 %
@Thickness 2.00 mm
Solar UV-A transmission factor, Darkened
 4.0 %
@Thickness 2.00 mm
Solar UV-A transmission factor, Heat Faded
 <= 0.10 %
@Wavelength 280 - 315 nm,
Thickness 2.00 mm
t(max), Heat Faded
 <= 0.10 %
@Wavelength 280 - 315 nm,
Thickness 2.00 mm
t(max), Darkened
 <= 0.10 %
@Wavelength 280 - 315 nm,
Thickness 2.00 mm
t(avg), Heat Faded
 <= 0.10 %
@Wavelength 280 - 315 nm,
Thickness 2.00 mm
t(avg), Darkened
 1.0 %
@Wavelength 315 - 350 nm,
Thickness 2.00 mm
t(max), Darkened
 1.5 %
@Wavelength 315 - 350 nm,
Thickness 2.00 mm
t(max), Heat Faded
 2.0 %
@Wavelength 380 - 500 nm,
Thickness 2.00 mm
t(moy), Darkened
 6.0 %
@Wavelength 380 - 500 nm,
Thickness 2.00 mm
t(moy), Heat Faded
 
Descriptive Properties
ColorClear to medium gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Corning FUSIBLE PHOTOBROWN EXTRA ™ Photochromic crown glass
Corning Unicrown Chemtemperable, UV absorbing crown glass
Corning PHOTOGRAY EXTRA™ Photochromic crown glass.
Corning PHOTOBROWN EXTRA™ Photochromic crown glass.
Corning PHOTOBROWN 16/45 High index photochromic crown glass

CCORN922 / 233333

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.