Appeel® LSR20D745 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad temperature range to a number of container materials including PET, PVC, PS and PP. Appeel® LSR20D745 is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene resins. Information provided by DuPont™ This former DuPont product line is now a Dow product line. |