MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Ryton® BR111 PPS, Glass fiber and mineral filled
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled

Material Notes: Glass fiber and mineral filled, enhanced mechanical and electrical

Ryton® BR111 is a natural-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outstanding chemical resistance, even at elevated temperatures.

Markets/Uses: Automotive / Fuel Systems / Sender Units; Automotive / Mechanical & Structural Parts / Brake Power Pistons

Applications: Automotive Applications

Features: Chemical Resistant; Good Electrical Properties; Good Strength

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.94 g/ccASTM D792
Water Absorption 0.020 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 cm/cm
@Thickness 3.20 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.0040 cm/cm
@Thickness 3.20 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 101ASTM D785
Hardness, Rockwell R 119ASTM D785
Tensile Strength 159 MPaASTM D638
Tensile Stress 165 MPaISO 527-2
Elongation at Break 1.1 %ASTM D638
 1.1 %ISO 527-2
Flexural Strength 241 MPaASTM D790
 255 MPaISO 178
Flexural Modulus 19000 MPaISO 178
 19300 MPaASTM D790
Compressive Strength 295 MPaASTM D695
Poissons Ratio 0.34ASTM E132
Izod Impact, Notched 75.0 J/m
@Thickness 3.18 mm
ASTM D256
Izod Impact, Unnotched 320 J/m
@Thickness 3.18 mm
ASTM D256
Izod Impact, Notched (ISO) 8.00 kJ/m²Notch A; ISO 180
Izod Impact, Unnotched (ISO) 24.0 kJ/m²ISO 180
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
Surface Resistance 1.00e+16 ohmASTM D257
Insulation Resistance 1.00e+10 ohm
@Temperature 90.0 °C
IEC 60167
Dielectric Constant 4.6
@Frequency 1e+6 Hz
ASTM D150
 4.7
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 18.0 kV/mmASTM D149
Dissipation Factor 0.0020
@Frequency 1000 Hz
ASTM D150
 0.0030
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 180 secASTM D495
Comparative Tracking Index 225 - 275 VUL 746
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 10.0 µm/m-°C
@Temperature 100 - 200 °C
ASTM E831
 15.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
ASTM E831
CTE, linear, Transverse to Flow 30.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
ASTM E831
 70.0 µm/m-°C
@Temperature 100 - 200 °C
ASTM E831
Thermal Conductivity 0.510 W/m-KASTM C177
Maximum Service Temperature, Air 220 - 240 °CUL Temperature Rating
Deflection Temperature at 1.8 MPa (264 psi) 265 °CUnannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 1.60 mm
 5VA
@Thickness 1.60 mm
Oxygen Index 65 %ASTM D2863
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorNatural Color
FormsPellets
ProcessingInjection Molding
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4404 / 280204

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.