MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC ULTEM EXUM0169 PEI Blend (Asia Pacific)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.

Information provided by SABIC Innovative Plastics for Asia Pacific.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.28 g/ccASTM D 792
Density 1.28 g/ccISO 1183
Moisture Absorption 0.0800 %
@Temperature 23.0 °C
50% RH; ISO 62
Water Absorption at Saturation 0.36 %
@Temperature 23.0 °C
ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC Method
Melt Flow 43 g/10 min
@Load 6.60 kg,
Temperature 337 °C
ASTM D 1238
 56 g/10 min
@Load 5.00 kg,
Temperature 360 °C
cm^3/10 min Melt Volume Rate; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 108ASTM D 785
Tensile Strength at Break 80.0 MPa5 mm/min; ISO 527
 85.0 MPaType I, 5 mm/min; ASTM D 638
Tensile Strength, Yield 98.0 MPa5 mm/min; ISO 527
 103 MPaType I, 5 mm/min; ASTM D 638
Elongation at Break 80 %Type I, 5 mm/min; ASTM D 638
 80 %5 mm/min; ISO 527
Elongation at Yield 7.0 %Type I, 5 mm/min; ASTM D 638
 7.0 %5 mm/min; ISO 527
Tensile Modulus 2500 MPa1 mm/min; ISO 527
 3210 MPa5 mm/min; ASTM D 638
Flexural Yield Strength 135 MPa2 mm/min; ISO 178
 145 MPa1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 3100 MPa2 mm/min; ISO 178
 3320 MPa1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched 32.0 J/m
@Temperature 23.0 °C
ASTM D 256
 35.0 J/m
@Temperature -30.0 °C
ASTM D 256
 2085 J/m
@Thickness 3.20 mm
Reverse Notched; ASTM D 256
Izod Impact, Unnotched NB
@Temperature -30.0 °C
ASTM D 4812
 NB
@Temperature 23.0 °C
ASTM D 4812
Izod Impact, Notched (ISO) 2.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
 2.00 kJ/m²
@Temperature 23.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 2.00 kJ/m²
@Temperature 23.0 °C
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
Instrumented Impact Total Energy 8.00 J
@Temperature -20.0 °C
ASTM D 3763
 48.0 J
@Temperature 23.0 °C
ASTM D 3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmASTM D 257
Surface Resistance 1.60e+17 ohmASTM D 257
Dissipation Factor 0.0061
@Frequency 1e+6 Hz
ASTM D 150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 55.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
 60.0 µm/m-°C
@Temperature -40.0 - 150 °C
ASTM E 831
CTE, linear, Transverse to Flow 55.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
 60.0 µm/m-°C
@Temperature -40.0 - 150 °C
ASTM E 831
Deflection Temperature at 1.8 MPa (264 psi) 168 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
 173 °C
@Thickness 3.20 mm
unannealed; ASTM D 648
 178 °C
@Thickness 6.40 mm
unannealed; ASTM D 648
Vicat Softening Point 192 °CRate B/50; ASTM D 1525
 192 °CRate B/50; ISO 306
 195 °CRate B/120; ISO 306
Glass Transition Temp, Tg 200 °C

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI48622 / 189707

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.