MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LG Chemical LUPOY 1201-10P Polycarbonate, Injection Molded
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: Introduction: LUPOY PC 1201-10P resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.

Main Characteristics: FDA1, Medium viscosity, Good mold release

Applications: Toys, Food utensils, Packaging applications

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D792
Water Absorption 0.15 %
@Time 86400 sec
ASTM D570
Moisture Absorption at Equilibrium 0.32 %50% RH; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmASTM D955
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 73ASTM D785
Hardness, Rockwell R 118ASTM D785
Tensile Strength, Ultimate 71.0 MPaASTM D638
Tensile Strength, Yield 612 kg(f)/cm²50mm/min; ASTM D638
Elongation at Break 150 %ASTM D638
Elongation at Yield 6.0 %ASTM D638
Tensile Modulus 2410 MPaASTM D638
Flexural Strength 96.0 MPaASTM D790
Flexural Modulus 24600 kg(f)/cm²ASTM D790
Izod Impact, Notched 92.5 kg-cm/cm
@Thickness 3.20 mm
0.25 mm notch; ASTM D256
Izod Impact, Unnotched NBASTM D256
Dart Drop, Total Energy 87.0 J
@Thickness 3.20 mm
203 m/min; ASTM D 3763
Abrasion 45
@Load 1.00 kg,
# of Cycles 500
% change in haze; Taber, CS-10 F wheel; ASTM D1044
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+17 ohm-cmdry; ASTM D 257
Dielectric Constant 3.0
@Frequency 60 Hz
ASTM D 150
Dielectric Strength 420 V/milASTM D 149
Dissipation Factor 0.0010
@Frequency 60 Hz
ASTM D 150
Comparative Tracking Index 250 V
@Thickness 2.00 mm
IEC 112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 68.0 µm/m-°C
@Temperature -40.0 - 82.0 °C
ASTM D 696
Hot Ball Pressure Test >= 125 °CIEC 598-1
Deflection Temperature at 0.46 MPa (66 psi) 144 °CAnnealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 128 °CUnannealed; ASTM D648
 141 °CAnnealed; ASTM D648
Vicat Softening Point 149 °C
@Load 5.00 kg
50°C/h; ASTM D1525
Oxygen Index 26 %ASTM D 2863
Glow Wire Test 850 °C
@Thickness 2.00 mm,
Time 5.00 sec
IEC 695-2-1
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.586ASTM D542
Haze 0.70 - 1.5 %ASTM D1003
Transmission, Visible 89 %ASTM D1003
 
Descriptive Properties
Average Extent of Burning25 mmASTM D 635

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLHCHEM9717 / 239241

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.