Description: APJAC05 is a black high density polyethylene compound suitable for jacketing. It contains 2.5% well dispersed carbon black in order to ensure excellent weathering resistant. Antioxidant is added to obtain excellent long term properties. Specification: ASTM D1248 / Type ? / class C / category 5 / grade J5 - IEC 60502:ST7 - IEC 60840:ST7 - IEC 60708 Special features: - Outstanding UV resistance
- Termite resistance
- Low water permeability
- Excellent environmental stress crack resistance
- Oil resistance I & II, according to UL 1072
Information provided by Abhar Polymer Compounds |