MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Pressure Seal 101-64 Santoprene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes:

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.970 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 64
@Temperature 100 °C,
Time 86400 sec
ASTM D2240
 64
@Temperature 100 °C,
Time 605000 sec
ASTM D2240
 64
@Temperature 125 °C,
Time 86400 sec
ASTM D2240
 64
@Temperature 125 °C,
Time 605000 sec
ASTM D2240
 64
@Temperature 150 °C,
Time 86400 sec
ASTM D2240
 65
@Temperature 125 °C,
Time 1.30e+6 sec
ASTM D2240
 65
@Temperature 100 °C,
Time 1.30e+6 sec
ASTM D2240
 66
@Temperature 100 °C,
Time 3.60e+6 sec
ASTM D2240
 66
@Temperature 150 °C,
Time 1.30e+6 sec
ASTM D2240
 66
@Temperature 125 °C,
Time 3.60e+6 sec
ASTM D2240
 67
@Temperature 150 °C,
Time 605000 sec
ASTM D2240
 68
@Temperature 100 °C,
Time 2.59e+6 sec
ASTM D2240
 70
@Temperature 125 °C,
Time 2.59e+6 sec
ASTM D2240
 72
@Temperature 150 °C,
Time 2.59e+6 sec
ASTM D2240
 73
@Temperature 150 °C,
Time 3.60e+6 sec
ASTM D2240
 64
@Time 5.00 sec
ASTM D2240
Tensile Strength 870 psiUnaged Control; ASTM D412
 1000 psiDie C; ASTM D412
 439 psi
@Temperature 150 °C,
Time 3.60e+6 sec
ASTM D412
 507 psi
@Temperature 150 °C,
Time 2.59e+6 sec
ASTM D412
 861 psi
@Temperature 100 °C,
Time 2.59e+6 sec
ASTM D412
 865 psi
@Temperature 100 °C,
Time 605000 sec
ASTM D412
 880 psi
@Temperature 100 °C,
Time 1.30e+6 sec
ASTM D412
 888 psi
@Temperature 125 °C,
Time 86400 sec
ASTM D412
 890 psi
@Temperature 100 °C,
Time 86400 sec
ASTM D412
 894 psi
@Temperature 150 °C,
Time 86400 sec
ASTM D412
 900 psi
@Temperature 100 °C,
Time 3.60e+6 sec
ASTM D412
 934 psi
@Temperature 125 °C,
Time 605000 sec
ASTM D412
 938 psi
@Temperature 125 °C,
Time 2.59e+6 sec
ASTM D412
 959 psi
@Temperature 150 °C,
Time 1.30e+6 sec
ASTM D412
 962 psi
@Temperature 125 °C,
Time 1.30e+6 sec
ASTM D412
 980 psi
@Temperature 125 °C,
Time 3.60e+6 sec
ASTM D412
 1011 psi
@Temperature 150 °C,
Time 605000 sec
ASTM D412
Elongation at Break 420 %Unaged Control; ASTM D412
 65 %
@Temperature 150 °C,
Time 3.60e+6 sec
ASTM D412
 167 %
@Temperature 150 °C,
Time 2.59e+6 sec
ASTM D412
 395 %
@Temperature 100 °C,
Time 2.59e+6 sec
ASTM D412
 404 %
@Temperature 125 °C,
Time 86400 sec
ASTM D412
 407 %
@Temperature 125 °C,
Time 2.59e+6 sec
ASTM D412
 409 %
@Temperature 150 °C,
Time 86400 sec
ASTM D412
 412 %
@Temperature 100 °C,
Time 1.30e+6 sec
ASTM D412
 414 %
@Temperature 100 °C,
Time 86400 sec
ASTM D412
 416 %
@Temperature 125 °C,
Time 605000 sec
ASTM D412
 421 %
@Temperature 100 °C,
Time 605000 sec
ASTM D412
 424 %
@Temperature 100 °C,
Time 3.60e+6 sec
ASTM D412
 427 %
@Temperature 125 °C,
Time 1.30e+6 sec
ASTM D412
 434 %
@Temperature 150 °C,
Time 1.30e+6 sec
ASTM D412
 446 %
@Temperature 125 °C,
Time 3.60e+6 sec
ASTM D412
 447 %
@Temperature 150 °C,
Time 605000 sec
ASTM D412
Elongation, Ultimate 400 %ASTM D412
Tensile Modulus 3.40 MPa
@Temperature 100 °C
Young's modulus; ASTM D797.89
 7.30 MPa
@Temperature 23.0 °C
Young's modulus; ASTM D797.89
100% Modulus 334 psiUnaged Control; ASTM D412
 340 psiASTM D412
 320 psi
@Temperature 150 °C,
Time 86400 sec
ASTM D412
 326 psi
@Temperature 100 °C,
Time 605000 sec
ASTM D412
 329 psi
@Temperature 125 °C,
Time 86400 sec
ASTM D412
 333 psi
@Temperature 100 °C,
Time 86400 sec
ASTM D412
 336 psi
@Temperature 100 °C,
Time 1.30e+6 sec
ASTM D412
 338 psi
@Temperature 100 °C,
Time 2.59e+6 sec
ASTM D412
 339 psi
@Temperature 125 °C,
Time 605000 sec
ASTM D412
 339 psi
@Temperature 100 °C,
Time 3.60e+6 sec
ASTM D412
 344 psi
@Temperature 125 °C,
Time 1.30e+6 sec
ASTM D412
 347 psi
@Temperature 125 °C,
Time 3.60e+6 sec
ASTM D412
 348 psi
@Temperature 150 °C,
Time 605000 sec
ASTM D412
 355 psi
@Temperature 150 °C,
Time 1.30e+6 sec
ASTM D412
 359 psi
@Temperature 125 °C,
Time 2.59e+6 sec
ASTM D412
 380 psi
@Temperature 150 °C,
Time 2.59e+6 sec
ASTM D412
Flexural Modulus 18.5 MPa0.5 in/min. Secant modulus, 1%; ASTM D 790
Tear Strength 58.0 pli
@Temperature 100 °C
ASTM D624
 140 pli
@Temperature 25.0 °C
ASTM D624
Compression Set 22 %
@Temperature 25.0 °C,
Time 79200 sec
ASTM D395, Method B
 34 %
@Temperature 100 °C,
Time 79200 sec
ASTM D395, Method B
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -76.0 °FASTM D746
 
Descriptive Properties
Tension Set0.1ASTM D412

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPRESL256 / 318466

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.