MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Jilin Xingyun Chemical XY-1 Dispersion and corrosion inhibitor for ethylene process water
Categories: Other Engineering Material

Material Notes: This product is a multi-functional additive, which can control a variety of material corrosion. It is also susceptible to absorbing water and plays an important role in anti-fouling/scaling and demulsification. It can disperse and remove the insoluble inorganic salt in the water to prevent the metal from scale formation and it can help not only to maintain the metal heat transfer effects but also can effectively eradicate the oil-in-water emulsion to reduce the oil content in the water; this product can also interfere with the electrochemical corrosive ion in the water and prevent corrosion by forming a film on the surface of metal.

Information provided by Jilin Xingyun Chemical Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 - 1.25 g/cc
pH >= 8.0
Kinematic Viscosity <= 100 cSt
 
Thermal PropertiesOriginal ValueComments
Solidus <= -5.00 °C
 
Descriptive Properties
Appearancecolorless or yellowish oily liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PJILINX025 / 317872

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.