45% glass fiber, for thick-wall parts (>3mm), heat stabilized Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0.125 inch (3 mm). Key properties of this structural resin are high heat deflection temperature, high flexural modulus, high tensile strength, excellent creep resistance, and low moisture absorption. - Black: AS-1145 HS BK 324 - Natural: AS-1145 HS NT Applications: Automotive Applications; Automotive Electronics; Automotive Under the Hood; Connectors; Fuel Lines; General Purpose; Housings; Industrial Applications; Industrial Parts; Lawn and Garden Equipment; Machine/Mechanical Parts; Metal Replacement; Power/Other Tools; Thick-walled Parts; Valves/Valve Parts Features: Chemical Resistant; Creep Resistant; Good Dimensional Stability; Good Stiffness; Heat Stabilized; High Heat Resistance; High Strength; Low Moisture Absorption Injection notes: Storage: - Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Amodel® processing guide. Information provided by Solvay Specialty Polymers. |