LNP THERMOCOMP D551 (or DF00A8P) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good impact performance, Non-Brominated & Non-Chlorinated Flame Retardant.Information provided by SABIC |