MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ALM PA 603-CF Nylon 12, 33% Carbon Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Carbon Fiber Filled

Material Notes: 33% Carbon-Fiber-Filled Nylon 12 optimized for a smooth surface finish without sacrificing feature details.

Highlights:

  • High-Detail Black Surface Finish
  • Good Stiffness and Mechanical Properties
  • Warping Resistance at Elevated Temperatures
Applications:
  • High-performance impact sports equipment and racing applications
  • Industrial applications with an HDT of ~177° C
  • Wind tunnel model testing

Information provided by Advanced Laser Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.410 g/ccASTM D1895
Density 1.10 g/ccSintered; ASTM D792
Particle Size 50 µmD50
 35 - 100 µmD10-D90
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 85.0 MPaXY; ASTM D638
Elongation at Break 4.0 %XY; ASTM D638
Tensile Modulus 7900 MPaXY; ASTM D638
Flexural Modulus 9170 MPaXY; ASTM D790
Izod Impact, Notched 84.0 J/mXY; ASTM D256
Izod Impact, Unnotched 161 J/mXY; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 179 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 173 °CASTM D648
 
Descriptive Properties
ColorDark Gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PALP9009 / 312344

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.